KOMPOSISI KIMIA
incoloy 625 coiled tubing capillary tubing
C | Cr | Ni | Fe | Mn | Si | Mo | Co | P | S | Ti | Nb + Ta | Al |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤ 0.1 | 20 – 23 | ≥ 58 | ≤ 5 | ≤ 0,5 | ≤ 0,5 | 8 – 10 | ≤ 1* | ≤ 0,015 | ≤ 0,015 | ≤ 0.4 | 3.15 – 4.15 | ≤ 0.4 |
(massa%)
*Yen ditemtokake
ASTM B444, ASME SB444, AMS 5581
Kanggo ASTM B444, ASME SB444, AMS 5581
kahanan | Kekuwatan Tensile | Kekuwatan Ngasilake | Elongation |
minimal, ksi | minimal, ksi | minimal,% | |
kelas 1 | 120 | 60 | 30 |
kelas 2 | 100 | 40 | 30 |
*Sifat kekuatan sing luwih dhuwur bisa diwenehake ing kondisi hardened kadhemen.
incoloy 625 coiled tubing capillary tubing
70°F | 200°F | 400°F | 600°F | 800°F | 1000°F | ||
---|---|---|---|---|---|---|---|
Kapadhetan | lbs/ing3 | 0.305 | - | - | - | - | - |
Ekspansi Termal | X10-6/°F | - | 7.1 | 7.3 | 7.4 | 7.6 | 7.7 |
Modulus elastik | 103 ksi | 30.1 | 29.6 | 28.7 | 27.8 | 26.9 | 25.7 |
Rasio Poisson | - | 0.278 | 0.28 | 0.286 | 0.29 | 0.295 | - |
Konduktivitas termal | Btu-in/h·ft2·°F | 68 | 75 | 87 | 98 | 109 | 139 |
Panas Spesifik | Btu/lb·°F | 0.098 | 0.102 | 0.109 | 0.115 | 0.122 | 0.118 |
Kekuwatan Ngasilake | ksi | 70 | 68 | 63 | 60 | 59 | 34 |
Kekuwatan Tensile | ksi | 140 | 134 | 130 | 129 | 129 | 88 |
incoloy 625 coiled tubing capillary tubing
PROSESDESKRIPSISteel MakingElectric Arc Furnace ngiring dening Vacuum Oxygen Decarburization (VOD) utawa Argon Oxygen Decarburization (AOD).Pembuatan Pipa.Bisa kasedhiya ing anil, solusi anil utawa kadhemen hardened.Kondisi anil kekuatan sing luwih dhuwur biasane digunakake ing layanan nganti 1100 ° F, dene kondisi anil solusi digunakake ing aplikasi ing ndhuwur 1100 ° F.
Wektu kirim: Jul-06-2023