Rega Paduan 276 Stainless Steel Coil Tubing
Komposisi Kimia Hastelloy C276
SIHE STAINLESS STEEL modern banget ing teknologi kanggo Pack Barang miturut Standar Internasional lan inovasi paling anyar.Kita nekanake akeh babagan Pengepakan lan label supaya nyedhiyakake produk Kualitas Premium kanggo Pelanggan Domestik lan Internasional.Hastelloy C276 Fittings kasebut kanthi teliti, dikempalken karo lapisan saka plastik foils lan Gelembung kebungkus lan kasebut kanthi teliti, diselehake ing kothak Kayu.
Mangga nelpon kita kanggo dipikir liyane ing-ambane nggunakake tambahan sing kalebu sawetara data resistance karat komparatif, media, konsentrasi lan suhu.Kanggo informasi luwih lengkap babagan Pipa lan Sistem Pipa SIHE STAINLESS STEEL, waca kaca pipa Hastelloy C276 lan tabung Hastelloy C276.
Hastelloy C276 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
| imbangan | 0,010 maks | 15.00 – 17.00 | 1.00 maks | 0,08 maks | 4.00 – 7.00 | 0,04 maks | 0,03 maks | 2,5 maks | 14.50 – 16.50 |
Hastelloy C276 Sifat Mekanik
Sifat Tensile Suhu Kamar Khas saka Material Annealed
Formulir produk | Tarik (ksi) | .2% Ngasilake (ksi) | Elongation% |
Paduan C276 Bar | 110.0 | 52.6 | 62 |
Alloy C276 Plate | 107.4 | 50.3 | 67 |
Paduan C276 Lembar | 115.5 | 54.6 | 60 |
Alloy C276 Tube & Alloy C276 Pipa | 105.4 | 45.4 | 70 |
Hastelloy C276 Titik Lebur
Sifat Fisik | °F | Unit Inggris | °C | Unit Metrik |
Kapadhetan | 72 | 0,321 lb./in (3) | 22 | 8,89 g/cm(3) |
Lebur Range | 2415- | 1323- | ||
listrik | 75 | 51 mikrohm-ing. | 24 | 1,30 mikrohm-m |
Koefisien Tegese | 75-200 | 6,2 microin./in.-°F | 24-93 | 11,2 X 10(-6)m/mK |
75-400 | 6,7 microin./in.-°F | 24-204 | 12,0 X 10(-6)m/mK | |
75-600 | 7,1 microin./in.-°F | 24-316 | 12,8 X 10(-6)m/mK | |
75-800 | 7,3 microin./in.-°F | 24-427 | 13,2 X 10(-6)m/mK | |
75-1000 | 7,4 microin./in.-°F | 24-538 | 13,4 X 10(-6)m/mK | |
75-1200 | 7,8 microin./in.-°F | 24-649 | 14,1 X 10(-6)m/mK | |
75-1400 | 8,3 microin./in.-°F | 24-760 | 14,9 X 10(-6)m/mK | |
75-1600 | 8,8 microin./in.-°F | 24-871 | 15,9 X 10(-6)m/mK | |
75-1700 | 8,9 microin./in.-°F | 24-927 | 16,0 X 10(-6)m/mK | |
Thermal | -270 | 50 Btu-in/ft²-jam-°F | -168 | 7,2 W/mK |
-100 | 60 Btu-in/ft²-jam-°F | -73 | 8,6 W/mK | |
0 | 65 Btu-in/ft²-jam-°F | 32 | 9,4 W/mK | |
100 | 71 Btu-in/ft²-jam-°F | 38 | 10,2 W/mK | |
200 | 77 Btu-in/ft²-jam-°F | 93 | 11,1 W/mK | |
400 | 90 Btu-in/ft²-jam-°F | 204 | 13,0 W/mK | |
600 | 104 Btu-in/ft²-jam-°F | 316 | 15,0 W/mK | |
800 | 117 Btu-in/ft²-jam-°F | 427 | 16,9 W/mK | |
1000 | 132 Btu-in/ft²-jam-°F | 538 | 19,0 W/mK | |
1200 | 145 Btu-in/ft²-jam-°F | 649 | 20,9 W/mK | |
1400 | 159 Btu-in/ft²-jam-°F | 760 | 22,9 W/mK | |
1600 | 173 Btu-in/ft²-jam-°F | 871 | 24,9 W/mK | |
1800 | 185 Btu-in/ft²-jam-°F | 982 | 26,7 W/mK | |
2000 | 195 Btu-in/ft²-jam-°F | 1093 | 28,1 W/mK |
Hastelloy C276 Setara
STANDAR | UNS | WERKSTOFF NR. | AFNOR | EN | JIS | BS | GOST |
Hastelloy C276 | N10276 | 2.4819 | – | NiMo16Cr15W | NW 0276 | – | ХН65МВУ |
Spesifikasi Produk
ASTM B622, B829 / ASME SB622, SB829 / NACE MR0175
Ukuran Range
Diameter njaba (OD) | Kekandelan tembok |
.250”–.500” | .035”–.065” |
Tabung anil sing kadhemen lan padhang.
Syarat Kimia
Paduan C276 (UNS N10276)
Komposisi%
Ni nikel | Cr Kromium | Mo Molybdenum | Fe wesi | W Tungsten | C Karbon | Si silikon | Co kobalt | Mn Mangan | V Vanadium | P Fosfor | S belerang |
57,0 min | 14.5–16.5 | 15.0–17.0 | 4.0–7.0 | 3.0–4.5 | 0,010 maks | 0,08 maks | 2,5 maks | 1.0 maks | 0,35 maks | 0,04 maks | 0,03 maks |
Toleransi dimensi
OD | OD Toleransi | Toleransi Tembok |
.250"–.500" | +.004”/-.005” | ± 15% |
Sifat Mekanik
Kekuwatan Ngasilake: | 41 ksi min |
Kekuwatan tarik: | 100 ksi min |
Elongation (min 2"): | 40% |