316L stainless steel 6*0.6 mm coiled/pipa kapiler
DESKRIPSI:
316L stainless steel 6*0.6 mm coiled/pipa kapiler
Tipe 316 Stainless Steel yaiku baja tahan karat kromium nikel austenitik sing ngemot molibdenum.Tambahan iki nambah resistance karat umum, nambah resistance kanggo pitting saka solusi ion klorida, lan menehi tambah kekuatan ing suhu munggah pangkat.Properties padha karo Tipe 304 kajaba alloy iki rada kuwat ing suhu munggah pangkat.Ketahanan korosi luwih apik, utamane marang asam sulfat, hidroklorat, asetat, format lan tartarat;asam sulfat lan klorida alkalin.Stainless Steel Tipe 316L minangka versi karbon ekstra-rendah saka Tipe 316 sing nyilikake udan karbida sing mbebayani ing zona sing kena panas nalika ngelas.
FORMULIR PRODUK:
316L stainless steel 6*0.6 mm coiled/pipa kapiler
Lembaran, Strip, tubing, pipa
SPESIFIKASI:
316L stainless steel 6*0.6 mm coiled/pipa kapiler
ASTM A240, A666
APLIKASI KHAS:
316L stainless steel 6*0.6 mm coiled/pipa kapiler
manifold exhaust, bagean tungku, penukar panas, peralatan farmasi lan fotografi, tutup katup lan pompa, peralatan kimia, digester, tangki, evaporator, pulp, kertas lan peralatan pangolahan tekstil, bagean sing kena ing atmosfer laut lan pipa.
KOMPOSISI KIMIA: ASTM A240, A666
316L stainless steel 6*0.6 mm coiled/pipa kapiler
unsur | Tipe 316 | Tipe 316L |
---|---|---|
Karbon | 0,08 maks. | 0,030 maks. |
Mangan | 2.00 maks. | 2.00 maks. |
belerang | 0,030 maks. | 0,030 maks. |
Fosfor | 0,045 maks. | 0,045 maks. |
silikon | 0,75 maks. | 0,75 maks. |
Kromium | 16.0 – 18.0 | 16.0 – 18.0 |
nikel | 10.00 – 14.00 | 10.00 – 14.00 |
Molybdenum | 2.00 – 3.00 | 2.00 – 3.00 |
Nitrogen | 0.10 maks. | 0.10 maks. |
316L stainless steel 6*0.6 mm coiled/pipa kapiler
SIFAT MEKANIKAL: ASTM A240
Jinis | Kekuwatan Ngasilake 0,2% offset (KSI) | Kekuatan Tarik (KSI) | % Elongation (2″ Gauge dawa) |
---|---|---|---|
316 | 30 min. | 75 min. | 40 min. |
316L | 25 min. | 70 min. | 40 min. |
SIFAT FISIK:
Kapadhetan (lb./ in^2) @ RT | 0.29 | |
---|---|---|
Modulus Elastisitas ing Tegangan (psi x 10^6) | 28.0 | |
Kalor Spesifik (BTU/o F/lb.) | 32 kanggo 212 of | 0.12 |
Konduktivitas Termal (BTU/jam/ft^2/ft) | 212oF | 9.4 |
932oF | 12.4 | |
Rata-rata Koefisien Ekspansi Termal (ing. x 10^-6 per o F) | 32 kanggo 212oF | 8.9 |
32 kanggo 600oF | 9.0 | |
32 kanggo 1.000oF | 9.7 | |
32 kanggo 1.200oF | 10.3 | |
Resistivitas listrik (mikro ohm - cm) | ing 70oF | 29.4 |
Rentang Titik Lebur (oF) | 2500 – 2550 |